Faster dual-material printing, from wax to PEEK
The speed of an Epitum printer comes from the moments other machines waste: the nozzle switch, the wipe tower, the empty travel moves. Around that sit a 430 °C hot end, a 150 °C bed, an actively heated 90 °C chamber and supports that come off cleanly.

The speed is in the nozzle switch
A dual-material part changes nozzles thousands of times. On a conventional dual extruder every change means parking, re-heating and purging onto a wipe tower. JetSmart™ swaps the active nozzle in under half a second, seals the idle one with a mechanical valve so it cannot drip, and needs no tower at all.
- < 0.5 s nozzle swap, alignment repeatable to < 1 µm
- No wipe tower — no wasted material, no tower time on every layer
- Hot Swap mode — if one nozzle clogs or runs out, the other, loaded with the same material, carries on
- One print head, not IDEX — two nozzles on one carriage, switched by a valve
15 hours saved on a single part
| 300 mm dual-material part, 0.1 mm layers | Epitum JL · JetSmart™ | Conventional dual extruder |
|---|---|---|
| Material change | < 0.5 s nozzle swap, about 5 s per full change | About 40 s: park, re-heat, purge |
| Wipe / prime tower | None — a valve seals the idle nozzle | Printed on every layer |
| Active printing | 28.8 h | 24.6 h |
| Time spent changing materials | 3.2 h | 22.4 h |
| Total print time | 32 h | 47 h |
Manufacturer’s example: a 300 mm tall dual-material model printed at 0.1 mm layers.
Fast moves on a frame built for heavy, full-volume parts
A 360 × 360 × 610 mm volume holds about 79 liters — a solid nylon part that size would weigh around 90 kg. The machine is built for that load first and for speed second.
- Own electronics — an ARM Cortex-M4 motion board, a dedicated print-head controller and a Raspberry Pi interface board, all designed by Epitum
- Own firmware, written from scratch rather than adapted from Marlin, Klipper or RepRap
- 3 mm steel frame, steel linear rails on X/Y and cylindrical steel guides on Z
- Speed modes — pick a preset at the printer; the same print file runs faster or slower without re-slicing
| Before the speed update | Current firmware | |
|---|---|---|
| Travel speed (X/Y) | up to 150 mm/s | up to 500 mm/s |
| Acceleration (X/Y) | up to 2,000 mm/s² | up to 7,000 mm/s² |
| Motor driver modes | stealthChop | stealthChop + spreadCycle |
| Test print: technical box | 4 h 20 min | 1 h 45 min |
| Test print: ABS cover | 6 h | 2 h 30 min |
Test prints are the manufacturer’s own measurements. Print speed itself is set per material — typically 150–200 mm/s for rigid plastics and 20–40 mm/s for flexibles such as TPU; the gain comes from travel moves and acceleration.
From casting wax to PEEK on one printer
The 430 °C hot end covers the whole range; the chamber is set per material profile — off for wax, 90 °C for nylon and PC.
| Range | Materials | What to expect |
|---|---|---|
| Casting patterns | Casting wax, PMMA | Patterns for lost-wax investment casting; chamber heating off or low |
| Everyday | PLA, PETG, TPU, HIPS | Prototypes, fixtures, flexible parts |
| Engineering | ABS, ASA, PC, PA6 / PA12 / PA66, PP | Functional parts; the 90 °C chamber keeps large parts from warping |
| Composites | ABS-CF, PA-CF, PC/PBT-GF, PPS-CF | Stiff, light parts and metal replacement; standard nozzles are wear-resistant |
| High-performance | PEEK, PEKK, PEI, PPSU | 430 °C nozzle and 150 °C bed; plan for annealing and smaller parts |
90 °C, heated from the top down
Most heated chambers warm the air from below and wait for the whole volume to catch up. Epitum puts two 400 W PTC heaters at the upper rear and side of the chamber, and fans pull air through them and back around the part. Warm air rises anyway — starting at the top gets the print zone stable sooner and keeps the upper layers of a 610 mm part as warm as the first ones.
- Up to 90 °C (194 °F), set per material profile
- Self-regulating PTC heaters with a thermal fuse and a separate controller
- 150 °C heated bed adds steady heat from below
- Built-in drying mode — e.g. PVA at 90 °C for 3 hours inside the chamber

Where 90 °C sits among heated chambers
| Chamber class | How it is heated | What it prints well |
|---|---|---|
| Enclosure only | Heat from the bed and hot end | PLA, PETG; ABS with effort |
| Passive chamber | Warm air from the bed, no thermostat | ABS, PC/ABS, some filled nylons |
| Active, 60–70 °C | Dedicated heater, basic control | ABS, fiber-filled grades, PC/ABS |
| Active, 90 °C — Epitum | Two 400 W PTC heaters, recirculating fans, thermostat | Unfilled PA6 / PA12, PC, PPS, CF/GF composites; tall parts |
| Industrial, 150 °C+ | Insulated oven chamber | PEEK, PEKK, PEI at full size and crystallinity |
Why the chamber temperature matters: glass transition
| Material | Glass transition (Tg) | What a 90 °C chamber does |
|---|---|---|
| ABS / ASA | ≈ 100–105 °C | Chamber close to Tg — low internal stress, little warping |
| PC | ≈ 145–150 °C | Hot chamber needed for large parts; 90 °C keeps layers bonding |
| PA6 / PA12 (dry) | ≈ 40–60 °C | Chamber above Tg slows cooling and controls shrinkage |
| PPS | ≈ 85–90 °C | Chamber at Tg — the sweet spot for this semi-crystalline polymer |
| PEEK / PEI | ≈ 145 / 215 °C | Far above 90 °C — print smaller parts, anneal PEEK afterwards |
Approximate published values; Tg varies by grade, filler and moisture content.
EasySupport™ — supports that come off clean
On the dual-nozzle Epitum JL, the slicer builds supports from two materials in alternating layers with a buffer interface, so they release from the part instead of tearing.
| EasySupport™ BreakAway | EasySupport™ Soluble | |
|---|---|---|
| Removal | Snap off by hand | Soak in an alkaline bath, rinse |
| Post-processing | None | Rinse after soaking |
| Geometry | External overhangs | Internal channels, cavities, assemblies |
| Material range | ABS, PA, PC, composites | Wider, including high-temperature materials |
| Speed and cost | Fast, low cost | Medium; slicer cuts support material use |
Case study: replacing a CNC-machined aluminum part
A custom motorcycle fork mount, previously machined from aluminum, printed in glass-filled ABS with EasySupport™ Soluble. The slicer’s support geometry used 58% less soluble material and the surfaces needed no sanding.
| Motorcycle fork mount, ABS-GF + soluble support | Conventional supports | EasySupport™ Soluble |
|---|---|---|
| Cost per part | $36.32 | $28.01 (−23%) |
| 100 parts | $3,632 | $2,801 |
| 1,000 parts | $36,320 | $28,010 |
| Soluble support used | — | 58% less (49 kg saved per 1,000 parts) |
Manufacturer’s case study; client confidential.
Printoformer slicer
- Tree supports — up to 30% less support material on smaller parts; solid supports stay the default for tall, heavy parts, where tree supports can tip over
- Gyroid sub-interface layers for easier separation between support and part
- Support blockers — draw a volume where no supports are generated
- Minimum wall thickness shown on model load; seam visualization in the toolpath view
- Network printing — monitor and control every printer on the LAN from one window
Frequently asked questions
Is the Epitum JL an IDEX printer?
No. IDEX machines carry two independent print heads on separate carriages. The JL has one print head with two nozzles: JetSmart™ moves the active nozzle into place in under 0.5 s while a mechanical valve seals the idle one, so no wipe tower is needed.
Does 500 mm/s mean every part prints at 500 mm/s?
No — and we do not claim it. 500 mm/s is the travel speed for non-printing moves, with acceleration up to 7,000 mm/s². Print speed is set per material: typically 150–200 mm/s for rigid plastics, 20–40 mm/s for flexibles such as TPU. Faster travel and acceleration are what cut the time on real jobs.
Can a 90 °C chamber print PEEK?
It can print PEEK, PEKK and PEI with the 430 °C nozzle and the 150 °C bed, but a 90 °C chamber is below what these polymers ideally want, so large parts are harder and PEEK is usually annealed after printing. Read the PEEK guide before you plan a big PAEK part.
Which support type should I choose — breakaway or soluble?
Breakaway EasySupport™ is fastest: snap the supports off by hand, no chemicals. Soluble supports handle internal channels, enclosed cavities and high-temperature materials, but need a wash bath. Both use the second nozzle, so they run on the Epitum JL rather than the single-nozzle Epitum L.
See JetSmart™ print your part
Send us a model — a dedicated engineer will follow up within one business day.