ASA filament: print settings and ASA vs ABS for outdoor parts

ASA (acrylonitrile styrene acrylate) prints and behaves much like ABS, but it is built to live outdoors. This guide explains why it weathers better, what published UV-aging tests actually show, and the typical settings manufacturers recommend.

$63.98 ASA UV729 · 1 kg spool · USD
Order / Request a quote

ASA vs ABS — and when to choose ASA

Both are styrene-acrylonitrile plastics toughened with a rubber phase. In ABS that rubber is polybutadiene, whose carbon–carbon double bonds are attacked by UV light and oxygen; outdoors, ABS parts tend to yellow and lose toughness. ASA replaces it with a saturated acrylate rubber, so the surface holds up far better in sun and rain. Its stiffness, heat resistance and printability are close to ABS.

Choose ASA for any part that lives outdoors or under strong light. For indoor parts, ABS does the same job; if you need more heat or impact resistance, look at polycarbonate.

What the weathering data shows. In one FDM manufacturer's published test, natural-color ASA coupons were cycled for 1,000 hours in a QUV chamber per ASTM G154 (UV at 60 °C alternating with condensation at 50 °C). Upright tensile coupons kept about 97% of their stress at break (30.5 → 29.5 MPa), and the plaques showed only minor color change, while an ABS-based composite in the same test yellowed noticeably. Pigments affect color retention, so qualify the actual color you will use.

Typical properties

PropertyTypical rangeTest method
Density1.07–1.13 g/cm³ISO 1183 / ASTM D792
Tensile strength, printed XY32–44 MPaISO 527 / ASTM D638
Tensile strength, printed Z28–32 MPaISO 527 / ASTM D638
Tensile modulus2.1–2.4 GPaISO 527 / ASTM D638
Elongation at break, XY6–7 %ISO 527 / ASTM D638
Heat deflection, 1.8 MPa98–100 °CISO 75 / ASTM D648
Heat deflection, 0.45 MPa102–103 °CISO 75 / ASTM D648
Glass transition98–104 °CDSC
UV aging, 1,000 h QUV≈ 97 % break strength retained (one published test)ASTM G154

Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).

Typical print settings

Nozzle temperature235–265 °C
Build plate90–110 °C; textured PEI, PC, or glass with adhesive
ChamberClosed and heated (Epitum: up to 90 °C)
Print speed50–200 mm/s; slower outer walls
Part coolingOff; brief low fan for bridges only
Drying≈ 70 °C · 6–8 h; store sealed with desiccant
NozzleBrass is fine, ≥ 0.4 mm

Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.

Like ABS, ASA warps on large parts. Close the chamber, preheat it, and print the first layer slowly; one manufacturer prints its ASA test specimens in a 90 °C environment. For bed surfaces and adhesives, follow the ABS first-layer adhesion guide.

Which Epitum: JL or L

The Epitum L ($8,299) covers most ASA work: signage, housings and brackets printed in one material. Its heated chamber (up to 90 °C) is what keeps long, flat outdoor parts from curling, and the 360 × 360 × 610 mm volume fits tall enclosures in one piece.

The Epitum JL ($9,899) earns its place on parts with internal channels or enclosed overhangs: run ASA in one nozzle and VXL111 soluble support — which lists ASA — in the other. JetSmart™ seals the idle nozzle with a mechanical valve and switches in under 0.5 s, with no wipe tower.

Applications

  • Outdoor enclosures, junction boxes, sensor and camera housings
  • Automotive exterior trim prototypes, mirror and grille parts
  • Signage, garden and agricultural equipment parts
  • Jigs and fixtures used under strong shop lighting or near windows

Troubleshooting and tips

  • Warped corners. Preheat the chamber, raise the bed toward 110 °C, add a brim.
  • Layer splits on tall parts. Fan off, chamber closed, nozzle 5–10 °C hotter.
  • Dull or rough finish. Usually moisture — dry the spool and keep it sealed with desiccant.
  • Fumes. ASA releases styrene while printing; use an enclosed printer in a ventilated room or filtered exhaust.
  • Design for sun. Dark parts in direct sun run much hotter than the air; keep that margin against the heat-deflection temperature.

Available from MG World Tech: ASA UV729, 1 kg spool, $63.98. Order or request a quote →

Frequently asked questions

Is ASA better than ABS?

For outdoor parts, yes: its acrylate rubber resists UV far better than the butadiene rubber in ABS. Indoors the two are close in strength and heat resistance, so ABS does the job.

How long does ASA last outdoors?

No datasheet gives a service life in years. In one published accelerated test, natural ASA kept about 97% of its break strength after 1,000 hours of ASTM G154 cycling. Test your color and design in your own conditions.

Does ASA need an enclosure?

Yes, for parts of any size. Manufacturers list a closed chamber as required; a heated chamber further reduces warping and layer splitting.

What temperature do you print ASA at?

Typically 235–265 °C at the nozzle and 90–110 °C on the bed, part cooling off, inside a closed chamber.