Materials guide · Specialty

Wax filament for lost-wax casting: print settings and workflow

Wax and wax-like filaments let an FDM printer make patterns for lost-wax (investment) casting without injection tooling. They print cool, melt out of the mold like paraffin and are very different from ordinary plastics. This guide compiles what manufacturers and researchers have published, including where that data is thin.

What casting wax filament is — and when to choose it

In lost-wax casting a pattern is attached to a sprue, surrounded by plaster-like investment or a ceramic shell, and then removed by heat so that molten metal can fill the cavity. Traditionally the pattern is injection-molded or carved wax. A wax filament replaces the mold: you print the pattern directly, which suits one-offs, jewelry, dental-style small parts and engineering prototypes that will later be cast in aluminum, bronze or steel.

“Wax filament” covers two different things. Some products are wax-like thermoplastics that soften and flow out of a hot mold the way paraffin does; one maker describes its filament as a wax-alike thermoplastic that avoids a separate high-temperature burnout. Others, such as PVB-based casting filaments, are plastics formulated to burn out cleanly and need a real kiln. Research on true wax filaments blends microcrystalline wax with polymers, because pure wax is too brittle and flows poorly. For clean burnout of a plastic pattern, see our PMMA and PVB casting-filament guide.

Typical properties

PropertyTypical rangeSource type
Density≈ 1.18 g/cm³ (one wax-alike filament)Retailer listing
Softening / pour point≈ 70–75 °C for research wax blendsResearch paper
Filament diameters1.75 mm and 2.85 mmRetailer listing
Cold behaviorBrittle at about 15 °C; bendable at 25–30 °CMaker instruction sheet
Mold temperature for melt-out≈ 250–270 °C (wax-alike filament)Maker, retailer
Residue after burnoutNot published for wax-alike filament—

Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).

Published data is thin: product pages, one instruction sheet and one research paper, no comparable datasheets. Verify on a test pattern.

Typical print settings

Nozzle temperature170–220 °C (sources disagree; Epitum reaches 430 °C)
Build plate20–40 °C
ChamberOff (Epitum: heating off or very low, not the 90 °C maximum)
Print speedModerate; no consistent published figure
Part coolingPer spool; casting filaments of other types print with the fan on
DryingNot required by the wax-alike makers; keep the spool at about 40 °C if brittle
NozzleBrass, 0.4 mm or larger

Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.

The two sources we found that state a nozzle range for the same wax-alike filament disagree: one instruction sheet says 175–190 °C with a bed of at most 20 °C, while a retailer listing says 200–220 °C with a bed around 40 °C. Start low and raise the temperature until the layers fuse. A wax pattern should never see a hot bed or a hot chamber.

These filaments are brittle when cold. One maker notes that its filament can snap when bent around small radii and that warming it helps (15 °C brittle, 25–30 °C bendable). Keep the filament path short and gentle and the room warm.

From pattern to metal: the casting workflow

  • Print the pattern. Add allowance for metal shrinkage in CAD as you would for any cast part.
  • Sprue and tree. Attach the pattern to a wax sprue or gate system, singly or as a tree.
  • Invest. Pour plaster-type investment around the tree (jewelry practice) or build a ceramic shell (engineering foundries). One maker also describes embedding the print in clay or concrete for permanent-mold work.
  • Remove the pattern. The filament maker's instructions call for heating the mold to roughly 250–270 °C in an oven or kiln, where the filament flows out like hot paraffin; the same maker says this is why no high-temperature kiln burnout is needed. That is the manufacturer's claim, so run a trial, and ask your foundry about residue. Plastic casting filaments instead burn out around 500–1,200 °C.
  • Cast and finish. Pour metal into the hot mold, then clean, cut sprues and polish.

Users: jewelers, dental and hobby casters, and prototype foundries.

Surface finishing

Layer lines are copied into the metal, so finish the wax pattern before investing. Makers of wax-like filaments publish little on this. In ordinary jewelry-wax practice, patterns are smoothed with light warmth or by gentle hand tools and fine abrasives, but test on a scrap: a low-melting pattern distorts easily.

Which Epitum printer: JL or L

Wax is on Epitum’s list of supported materials — the range runs from wax to PEEK on the same 430 °C hot end. For patterns, Epitum L is enough. Turn chamber heating off, because a wax-like filament softens at a temperature far below what the chamber can reach. The Epitum JL adds a second nozzle for a soluble support under overhangs; check material compatibility with the support maker first, as support filaments are specified for particular partner materials (see the soluble-support guide).

Troubleshooting and tips

  • Filament snaps. It is too cold or bent too sharply. Warm it and shorten the path.
  • Layers do not fuse. Raise the nozzle in 5 °C steps.

Not in our standard catalog. Talk to an engineer about your casting patterns: contact us →

Frequently asked questions

Is wax filament real wax?

Usually not entirely. Research papers show that pure wax is too brittle and flows poorly for printing, so filaments blend wax with polymers. Commercial wax-alike products are thermoplastics designed to melt out like paraffin.

Do I need a kiln for wax filament patterns?

One maker states its filament needs only a household oven at about 250 °C because it flows out like wax. Other casting filaments such as PVB need a real burnout kiln. Confirm with a test cast.

Can I print wax on a printer with a hot chamber?

Yes, but leave chamber heating off or low. A wax-like pattern softens far below the chamber's maximum, and a hot chamber would distort it.

What is the difference between wax and PMMA casting filament?

Wax-like filament leaves the mold as a liquid at a modest temperature. PMMA and PVB burn out at much higher temperatures and print harder. See the PMMA casting guide.

Related guides

Keep reading

All material guides →

Talk to an engineer about your casting patterns

Send us the drawing, the load case and the service temperature — we will tell you honestly whether the Epitum envelope fits the part.

Talk to an engineer