Materials guide · Engineering

How to 3D print nylon (PA6, PA12 and PA66)

Pure nylon is tough, abrasion-resistant and fatigue-resistant, and it is one of the least forgiving filaments to print. This guide covers unfilled PA6, PA12 and PA66: typical settings, why moisture and warping are the real problems, and how a heated chamber helps.

What nylon is — and when to choose it

Nylons are polyamides. PA6 and PA66 are strong and stiff but absorb a lot of water; PA12 has a longer hydrocarbon chain and takes up far less, which gives steadier dimensions. Published figures for filament make the difference clear: one PA6 datasheet lists about 3 % moisture at 23 °C and 50 % relative humidity and 9 % at saturation, and a generic PA datasheet lists 3.2 %. The makers of PA12 filament talk instead about dimensional stability. Water plasticizes nylon, so a part that is stiff off the printer can be noticeably softer after weeks in humid air.

Choose nylon for gears, bushings, clips, living hinges, jigs and wear parts where toughness and abrasion resistance matter. If you need stiffness instead, see our PA12 carbon-fiber and PA-CF guides; for glass-filled parts see PC/PBT-GF.

Typical properties

PropertyTypical rangeSource type
Melting pointPA12 ≈ 178 °C; copolymer ≈ 214 °C; PA6 ≈ 220 °CMaker pages, literature
Glass transition (dry)≈ 68 °C (one nylon copolymer)Retailer listing
Density1.01–1.13 g/cm³ISO 1183 / 1148
Tensile strength≈ 45–58 MPaISO 527
Elongation at break≈ 32–36 % to > 50 %ISO 527
HDT at 0.45 MPa≈ 85–135 °CISO 75
Moisture uptake, 23 °C / 50 % RH≈ 3 % (PA6, copolymers); PA12 much lowerISO 62
Moisture, saturation≈ 9 % (PA6)ISO 62

Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).

Grades differ widely: copolymers such as PA6/66 melt lower, and impact-modified blends are softer. The table spans the sources we found; check your spool's datasheet.

Typical print settings

Nozzle temperature220–280 °C (Epitum: up to 430 °C)
Build plate80–120 °C (low-warp grades 25–50 °C with glue)
Chamber40–90 °C, hotter for PA6 and large parts (Epitum: up to 90 °C)
Print speed35–60 mm/s
Part cooling0–10 % (some sheets: 20–50 %)
Drying70–80 °C · 4–12 h in a dedicated dryer
NozzleBrass or hardened steel, ≥ 0.4 mm

Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.

Nozzle temperatures are lowest for copolymers (about 235–260 °C), mid-range for PA12 (about 245–270 °C) and highest for PA6 (about 260–280 °C). For layer adhesion keep part cooling at zero to 10 %; one PA12 maker sets 0–10 %, a generic PA sheet allows 20–50 %.

Why the chamber matters. Nylon is semi-crystalline: it shrinks as it crystallizes, and a layer cooling in cold air pulls on the layers below it. The glass transition of dry nylon is low (one nylon copolymer lists 68 °C), so the aim is to keep the whole part in the warm zone near and above it while printing. Makers differ on how much is needed. A generic sheet allows room temperature to 40 °C, and one PA12 maker requires a closed, heated chamber. For large flat parts and PA6 we would treat an enclosed, warm chamber as the rule.

Epitum heats its chamber actively up to 90 °C, which covers these recommendations. Absorbed water also lowers the glass transition, so dry the filament before relying on any chamber temperature.

Drying and moisture

Dry before printing and print from a dry box. Published drying conditions range from 70 °C for 4 h (one PA12 maker) and 75–80 °C for 6–8 h (one PA6 maker) to 80 °C for at least 12 h (a generic sheet). Do not exceed about 100 °C, or the spool can deform. The Epitum printers have a built-in drying mode (chamber up to 90 °C), but the manual says it does not guarantee the required moisture level for every material, so use a dedicated filament dryer for nylon. Wet nylon pops, strings and prints with a rough surface and weak layers.

Which Epitum printer: JL or L

Epitum L handles single-material nylon parts. The Epitum JL adds a second nozzle, useful when a part needs a soluble support under overhangs; a generic nylon sheet lists PVA as a compatible support, and the soluble-support guide covers the options.

Applications

  • Gears, bushings and sliding or wear parts
  • Snap-fits, clips and living hinges
  • Jigs, fixtures and tool handles that see impact
  • Housings and brackets where toughness beats stiffness

Troubleshooting and tips

  • Warping and curling. Preheat the chamber, add a brim and keep drafts out. Large flat footprints warp first.
  • Adhesion. Nylon often needs glue or an adhesive sheet on PEI or glass; some makers specify PVA-type glue.
  • Bubbles and stringing. The spool is wet. Dry it again and feed from a sealed box.
  • Weak layers. Raise the nozzle temperature, slow down and reduce cooling.
  • Dimensions drift. Condition the part in the air it will live in, then measure.

Not in our standard catalog. Talk to an engineer about your nylon part: contact us →

Frequently asked questions

Why does my nylon warp so badly?

Semi-crystalline nylon shrinks as it cools and crystallizes, so cold air around the part curls it. A closed, preheated chamber, a hot bed, a brim and little part cooling all reduce it.

Is PA12 easier to print than PA6?

Usually yes. It takes up much less water and holds dimensions better, though makers still recommend a closed, heated chamber for it. PA6 is hotter to print and wetter.

Can I dry nylon in the printer's drying mode?

Use it as a helper, not as a replacement. The manual does not guarantee the moisture level for all materials, so dry nylon in a dedicated filament dryer.

What bed temperature does nylon need?

Typically 80–120 °C with glue on PEI or glass. Some warp-reduced grades are formulated for 25–50 °C; follow your spool.

Related guides

Keep reading

All material guides →

Talk to an engineer about your nylon part

Send us the drawing, the load case and the service temperature — we will tell you honestly whether the Epitum envelope fits the part.

Talk to an engineer