PEKK 3D printing: PEKK-A, PEKK-SC and how to print them

PEKK is the PAEK polymer many engineers try when PEEK fights them on the printer. It crystallizes more slowly, which helps layers bond and parts stay flat. This guide explains the grades, typical settings, annealing, and what to expect on an Epitum printer.

What PEKK is — and why it is often easier than PEEK

Polyether ketone ketone (PEKK) is a PAEK polymer made from two isomers: terephthalic (T) and isophthalic (I). The T:I ratio sets how fast it crystallizes and where it melts. Resin makers publish roughly three families. At 80:20 it crystallizes fast and melts near 358 °C. At 70:30 it crystallizes at a medium rate and melts near 332 °C. At 60:40 it crystallizes slowly, is almost amorphous and melts near 305 °C. The glass transition stays near 160–165 °C throughout.

Filament names follow this logic. PEKK-A (amorphous) is the 60:40 type: it prints clear amber, bonds well between layers and warps little. PEKK-SC and other slow- or semi-crystalline grades use a higher T content. They reach more crystallinity, heat resistance and chemical resistance, but ask for a hotter environment or an anneal. PEEK, by contrast, crystallizes so fast that cold layers stop fusing. In one published study, as-printed slow-crystallizing PEKK kept about 80 % of its in-plane strength through the layers. That gap is why PEKK is the friendlier PAEK. When PAEK is more than the job needs, PPS-CF is a cheaper route to heat and chemical resistance.

Typical properties

PropertyTypical rangeTest method
Glass transition (Tg)160–165 °CISO 11357 (DSC)
Melting point (Tm)≈ 305 °C (PEKK-A, 60:40) · ≈ 332 °C (70:30-type SC)ISO 11357 (DSC)
Tensile strength, XY85–115 MPaISO 527
Tensile modulus, XY2.7–3.6 GPaISO 527
Elongation at break5–10 %ISO 527
HDT≈ 150–175 °CISO 75
Max. use temperature≈ 150 °C amorphous · 250–260 °C crystallizedManufacturer rating
Density1.27–1.29 g/cm³ISO 1183
FlammabilityUL94 V-0UL94

Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).

Typical print settings

Nozzle temperature340–380 °C (Epitum: up to 430 °C)
Build plate110–160 °C (Epitum: up to 150 °C)
Chamber70–150 °C for PEKK-A; up to 150–170 °C in some guides (Epitum: up to 90 °C)
Print speed20–50 mm/s
Part coolingOff
Drying110–120 °C · 4–8 h
Nozzle430 °C-rated, ≥ 0.4 mm; hardened for carbon- or ceramic-filled grades

Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.

The Epitum hot end reaches 430 °C, well above typical PEKK nozzle ranges. The chamber is the honest limit. Epitum heats it actively to 90 °C, which sits inside the low end of what PEKK-A makers suggest but well below the 150–170 °C some PEKK makers list. Treat 90 °C as the amorphous route: print PEKK-A, or a slow-crystallizing grade kept amorphous, then crystallize it in an oven if the part needs the higher rating.

Which Epitum: JL or L

The Epitum L fits most PEKK work: one material, one nozzle, a 360 × 360 × 610 mm volume, and an end-of-filament sensor for long jobs. Choose the Epitum JL if you want a second material or a nozzle reserved for high-temperature polymers. Soluble supports for PAEK exist but are specialized high-temperature products; see the general soluble-support guide. We review PEKK parts individually. Size, wall thickness and service temperature decide whether the 90 °C envelope is enough.

Applications

  • Aerospace-style brackets, clips and ducting where flame, smoke and toxicity performance matters
  • Fluid-handling parts exposed to fuels, oils and solvents
  • Electrical insulators and housings near hot components
  • Fixtures for hot processes, after annealing

Troubleshooting and tips

  • Know your grade. PEKK-A and PEKK-SC differ in melting point and in how they respond to annealing. Use the profile and schedule written for your spool.
  • Warping on larger parts. Risk grows with footprint and height at a 90 °C chamber. Use a brim, round the corners, keep the door closed and preheat the chamber before the first layer.
  • Bed surface. Makers list PEI sheet or a high-temperature polymer adhesive on a 110–160 °C plate.
  • Anneal in steps. A published PEKK-A schedule holds 30 min at 160 °C, then holds at 200 °C (about 90 min in one study) until the part is uniformly tan, then cools slowly. One study annealed slow-crystallizing grades at 260 °C. Annealing above Tg can slump thin features and change dimensions slightly; support the part and measure a test piece first.
  • Bubbles or rough walls. The filament is wet; dry it and print from a dry box.

Not in our standard catalog. Talk to an engineer about your PEKK part: contact us →

Frequently asked questions

What is the difference between PEKK-A and PEKK-SC?

PEKK-A uses a high isophthalic ratio and stays essentially amorphous. It is the easiest to print and is rated near 150 °C unless annealed. PEKK-SC grades crystallize more and reach higher heat and chemical resistance, but need annealing or a hotter build environment.

Is PEKK easier to 3D print than PEEK?

Usually. It crystallizes more slowly and prints about 20–40 °C cooler at the nozzle, so layers fuse better and parts warp less. See our PEEK guide for comparison.

Can I print PEKK with a 90 °C chamber?

PEKK-A, yes, for small and medium parts; PEKK-A makers list chambers from about 70 °C. Large or tall parts and in-printer crystallization need a hotter machine. Ask us about your geometry.

Does PEKK need annealing?

Not to be usable. Annealing is optional for PEKK-A and raises its use temperature and chemical resistance. For full ratings it is the normal step.

Related guides

Keep reading

All material guides →

Talk to an engineer about your PEKK part

Send us the drawing, the load case and the service temperature — we will tell you honestly whether the Epitum envelope fits the part.

Talk to an engineer