PA-CF filament for metal replacement

High-fiber PA-CF — usually nylon 6 or 6/66 carrying 20 % or more chopped carbon fiber — is the stiffest mainstream FFF nylon and the usual first candidate when a machined aluminum part is to be printed instead. This guide covers what it can and cannot replace, and how to print it.

$152.98 PA 25 CF · 0.75 kg spool · USD
Order / Request a quote

What high-fiber PA-CF is — and what "metal replacement" really means

Most high-fiber PA-CF grades are based on PA6 or PA6/66 because those nylons are stiffer and more heat-resistant than PA12. Raising the fiber load to 20–25 % pushes the in-plane modulus toward 8–9 GPa when dry — roughly three times unfilled nylon — while density stays near 1.1–1.2 g/cm³. A PA12-based option exists too: it is less stiff but far less sensitive to humidity (see our PA12-CF guide).

Be precise about the aluminum comparison. Wrought 6061-T6 has a modulus near 69 GPa, about 310 MPa tensile strength and a density of 2.7 g/cm³. Per unit weight, dry printed PA-CF reaches only about a third of aluminum's stiffness and, in the best (XY) direction, roughly three-quarters of its strength — across layers, well under half. What PA-CF replaces is the over-designed aluminum part: fixtures, brackets, end-of-arm tooling and covers sized for machining convenience, not for load. Redesign with ribs and thicker sections rather than copying the metal geometry.

Typical properties

PropertyTypical range (dry)Test method
Base polymer / fiberPA6 or PA6/66, ≈ 20–25 % carbon fiber—
Tensile strength, XY100–110 MPaISO 527
Tensile strength, Z (layer bond)≈ 54 MPa (one published value)ISO 527
Tensile modulus, XYup to ≈ 8.6 GPaISO 527
Flexural strength / modulus, XY150–160 MPa / 5.5–7.0 GPaISO 178
Elongation at break, XY2–6 %ISO 527
Heat deflection, 0.45 MPa150–215 °CISO 75
Heat deflection, 1.8 MPa≈ 170 °C (one published value)ISO 75
Water absorption≈ 2.3–3.3 % at equilibriumEquilibrium, humid air
Density1.09–1.17 g/cm³ISO 1183

Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).

Dry vs. conditioned. PA6-based composites absorb roughly 2–3 % water at equilibrium, and water softens them. After a hot-water soak, one manufacturer's PA6-CF kept about half its tensile strength and under a third of its tensile modulus; another reports flexural modulus falling by about a third when conditioned. Size real parts on conditioned values, or keep them dry in service.

Typical print settings

Nozzle temperature240–300 °C
Build plate80–110 °C, glue or PA adhesive on PEI (some low-warp grades: 40–50 °C)
ChamberOptional for many grades; 30–80 °C improves layer bonding (Epitum: up to 90 °C)
Print speedTypically 40–100 mm/s
Part coolingOff to low
Drying80–100 °C · 4–12 h; store below 20 % RH
NozzleHardened steel or ruby, ≥ 0.4 mm (0.6 mm reduces clogging)

Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.

Dial in on a dried spool only: wet PA6 looks like a temperature problem (stringing, rough walls, weak layers) and misleads every adjustment. Begin around 280 °C and 50 mm/s, then raise the temperature in 5 °C steps if layer bonding is poor.

Which Epitum: JL or L

Epitum L is the production choice for metal-replacement parts in a single material. Its 360 × 360 × 610 mm volume takes full-size fixtures and tooling plates, the 90 °C heated chamber limits warping and helps layers bond on thick sections, and the end-of-filament sensor pauses a long, dense job when a spool runs out.

Pick the Epitum JL when the part needs soluble support — VXL111 lists PA among its partner materials — or when you want the composite in one nozzle and another material in the second. Both nozzles are wear-resistant as standard. The blocking valve seals the idle nozzle, so there is no wipe tower.

Applications

  • Production fixtures, drilling and assembly jigs, and CMM holding fixtures
  • End-of-arm tooling, gripper bodies and vacuum-cup mounts, where lower mass allows faster robot moves
  • Machine brackets, guards and sensor mounts formerly milled from aluminum plate
  • Housings and structural parts near engines or motors that run warmer than PA12 can take

Troubleshooting and tips

  • Drying is not optional. PA6-CF picks up moisture in hours of shop air. Dry before every job and print from a dry box; annealing in the oven also re-dries a part.
  • Anneal for stiffness and heat. Manufacturers commonly test after about 100 °C for 16 h. Support thin sections in the oven and expect slight shrinkage.
  • Plan for nozzle wear. At 20–25 % fiber, wear is faster than with lower-fill composites. Use hardened steel or ruby, check the orifice and line width periodically, and replace nozzles as consumables.
  • Orient for the load. Lay the main bending or tensile load along the layers; across layers the part is less than half as strong.
  • Avoid sharp internal corners. Elongation is about 2–6 %; fillets and gradual section changes do more for durability than extra walls.

Available from MG World Tech: PA 25 CF, 0.75 kg spool, $152.98. Order or request a quote →

Frequently asked questions

Can carbon fiber nylon replace aluminum?

For fixtures, brackets and tooling that are lightly loaded or over-designed in metal, often yes, at under half the weight. It does not match aluminum's absolute strength or stiffness, and printed parts are weaker across layers, so redesign the part for the plastic and test it.

Is PA6-CF or PA12-CF better?

PA6-based PA-CF is stiffer and more heat-resistant when dry. PA12-CF absorbs much less water, so it changes less in humid service. See the PA12-CF guide to compare.

How do you dry PA-CF filament?

Typically 80–100 °C for 4–12 hours in an oven or dryer that holds temperature evenly, then print from a sealed box with desiccant. Check your spool's datasheet for its limit.

Why is my PA-CF part weaker than the datasheet?

Usually moisture (in the filament or the part), loading across layers, or an unannealed part compared with annealed test bars. Datasheet values are measured on solid, ideally oriented specimens.

Related guides

Keep reading

All material guides →

Order PA 25 CF or ask an engineer

Tell us about the part — we will confirm the material, settings and the right Epitum printer, and send a quote.

Request a quote