What PC/PBT-GF is — and when to choose it
PC/PBT blends have long been molded for automotive exterior parts, power-tool housings and electrical enclosures. Polycarbonate is amorphous, tough and heat-resistant but prone to stress cracking in fuels, solvents and many cleaners; PBT is semi-crystalline and chemically robust but less tough. Resin suppliers describe the alloy as resistant to oils, fuels, lubricants and cleaning agents, with low moisture uptake and good dimensional stability. Chopped glass fiber then raises stiffness, reduces creep and cuts warping.
Choose it over plain PC when the part sees chemicals or needs more stiffness, and over carbon-fiber nylon when humidity or electrical insulation matters — glass fiber is not conductive and the alloy takes up little water. For a flame-retardant housing, look at PC/ABS V-0 instead.
Typical properties
| Property | Typical range | Basis |
|---|---|---|
| Composition | PC/PBT alloy + chopped glass fiber (content varies by grade) | PC/PBT-GF filament |
| Tensile strength, XY | 65–69 MPa | Glass-filled PC filaments, ISO 527 |
| Tensile strength, Z (layer bond) | ≈ 33 MPa (one published value) | Glass-filled PC filament, ISO 527 |
| Tensile modulus, XY | 4.8–5.4 GPa | Glass-filled PC filaments, ISO 527 |
| Flexural strength, XY | 102–113 MPa | Glass-filled PC filaments, ISO 178 |
| Elongation at break | ≈ 2.5 % (one published value) | Glass-filled PC filament, ISO 527 |
| Heat deflection, 1.8 MPa | 137–143 °C | Glass-filled PC filaments, ISO 75 |
| Heat deflection, 0.45 MPa | ≈ 150 °C, un-annealed (one published value) | PC/PBT-GF filament, ISO 75 |
| Density | ≈ 1.2–1.4 g/cm³ | Glass-filled PC and PC/PBT filaments |
Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).
Few filament makers publish full data for glass-filled PC/PBT, so several rows come from glass-filled PC filaments, the closest printed analogue. Treat them as orientation, not design values; the spool's own datasheet governs.
Typical print settings
| Nozzle temperature | 260–300 °C (glass-filled PC grades up to ≈ 330 °C) |
|---|---|
| Build plate | 90–120 °C, glue on textured PEI |
| Chamber | As warm as available; published 50–100 °C (Epitum: up to 90 °C) |
| Print speed | Typically 30–80 mm/s |
| Part cooling | Off to < 10 % for strength |
| Drying | 80 °C · 8–12 h, store sealed with desiccant |
| Nozzle | Hardened steel or ruby, ≥ 0.4 mm (0.5–0.6 mm preferred) |
Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.
Start around 270 °C, a 100–110 °C bed with an adhesive, and 40–60 mm/s. Glass-filled PC grades with a higher PC share run hotter, up to about 330 °C. If walls look dull and layers split, the filament is usually wet, not too cold.
Which Epitum: JL or L
Epitum L handles single-material production of housings, brackets and fixtures: the 430 °C hot end covers every published range, the 360 × 360 × 610 mm volume fits large enclosures, and the end-of-filament sensor pauses long jobs when a spool runs out. Be aware that some glass-filled PC filaments recommend chambers above the 90 °C Epitum maximum; for those, keep parts compact and use generous brims.
Choose the Epitum JL for undercuts and internal channels that need soluble support. VXL111 lists PC among its partner materials; on a PC/PBT blend, print an adhesion test first. JetSmart™ switches nozzles in under 0.5 s with no wipe tower.
Applications
- Electrical enclosures, connector shells and junction boxes where insulation and stiffness both matter
- Automotive brackets, covers and clips exposed to fuel, oil or washer fluid
- Power-tool and equipment housings that see lubricants and cleaning agents
- Production fixtures that must hold size in humid shops and survive solvent wipe-downs
Troubleshooting and tips
- Dry it, but not to death. Both PC and PBT degrade when melted wet, losing toughness. Dry at about 80 °C for 8–12 h; at least one manufacturer warns that overdrying can also harm the filament.
- Use a wear-resistant nozzle. Glass fiber is abrasive, like carbon fiber. Use hardened steel or ruby, 0.4 mm minimum; 0.5–0.6 mm reduces clogging.
- Keep the fan low. Off to under 10 % gives the strongest layers; a little more improves overhang surfaces at a cost in strength.
- Use an adhesive on the bed. Textured PEI with glue is the common recommendation; bare smooth PEI is discouraged by some makers.
- Expect a rougher surface. Glass leaves a matte, slightly fibrous finish. Plan for light sanding on sealing faces.
Available from MG World Tech: PC PBT GF, 0.75 kg spool, $68.31. Order or request a quote →
Frequently asked questions
Is glass fiber filament abrasive?
Yes. Glass fiber wears brass nozzles quickly, widening the orifice and changing extrusion width. Use a hardened-steel or ruby nozzle of 0.4 mm or larger.
What is PC/PBT used for?
In molding, mainly automotive exterior and under-hood parts, power-tool housings and electrical enclosures — parts that need toughness plus resistance to fuels, oils and cleaning agents. Glass-filled printed grades suit stiff housings, brackets and fixtures.
Glass fiber or carbon fiber filament?
Carbon fiber gives more stiffness per weight. Glass fiber is electrically non-conductive, usually lower in cost, and in a PC/PBT matrix far less sensitive to humidity than carbon-fiber nylon. For maximum stiffness, see our PA-CF guide.
Does PC/PBT-GF need a heated chamber?
A warm chamber helps on large or tall parts, and published recommendations run from about 50 to 100 °C. Epitum printers heat the chamber to 90 °C, which covers most of that range.