Materials guide · Composites

How to 3D print PPS carbon fiber (PPS-CF)

PPS-CF is polyphenylene sulfide filled with chopped carbon fiber: a stiff, chemically inert, inherently flame-resistant composite that keeps its shape far above the limits of nylon or PC. This guide compiles what manufacturers publish about it and how to print it on an industrial FFF machine.

$159.19 PPS CF 15 · 0.75 kg spool · USD
Order / Request a quote

What PPS-CF is — and when to choose it

Polyphenylene sulfide is a semi-crystalline high-temperature polymer. In molding it is the standard answer for pump housings, under-hood connectors and electrical parts, because it absorbs almost no water, resists fuels, acids, bases and most solvents, and is self-extinguishing without added flame retardants. Chopped carbon fiber makes the filament stiffer and cuts the shrinkage that would otherwise make PPS warp off the bed.

Choose PPS-CF over carbon-fiber nylon when moisture, chemicals or heat would soften a nylon part; choose it over PEEK when you need chemical and thermal stability but not PEEK's toughness or its 350 °C+ processing. The price is brittleness: elongation at break is typically 1–2 %, so PPS-CF is for stiff, hot, chemically exposed parts — not for clips, hinges or impact loads.

Typical properties

PropertyTypical rangeTest method
Fiber content≈ 10–15 % carbon fiber (by weight)—
Tensile strength, XY59–87 MPaISO 527
Tensile strength, Z (layer bond)24–32 MPaISO 527
Tensile modulus, XY5.4–8.2 GPaISO 527
Flexural strength, XY94–142 MPaISO 178
Elongation at break, XY1.2–1.8 %ISO 527
Heat deflection, 0.45 MPa250–265 °CISO 75
Heat deflection, 1.8 MPa130–235 °C (grade- and anneal-dependent)ISO 75
Glass transition / melting≈ 98–100 °C / 280–284 °CDSC
Water absorption0.05–0.23 %Saturation, 55–70 % RH
Density1.26–1.29 g/cm³ISO 1183

Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).

Note how far apart the published heat-deflection values are at 1.8 MPa: the result depends on the grade and on whether the specimen was annealed (crystallized) before the test. Use the 0.45 MPa value only for lightly loaded parts.

Typical print settings

Nozzle temperature310–350 °C
Build plate80–120 °C, adhesive (glue) on PEI
ChamberRoom temperature to 90 °C depending on grade (Epitum: up to 90 °C)
Print speedTypically 30–100 mm/s; slower improves layer bonding
Part coolingOff to 40 %
Drying100–140 °C · 4–12 h, stored below 20 % RH
NozzleHardened steel or other wear-resistant, ≥ 0.4 mm (0.6 mm preferred)

Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.

Start mid-range — around 320–330 °C and 40–60 mm/s — and print a tensile bar standing on end before a real part. If layers split, raise the nozzle temperature or slow down before you touch anything else; if the corners lift, add brim and raise the bed rather than the fan.

Which Epitum: JL or L

Both machines reach 430 °C at the nozzle and heat the chamber to 90 °C, which covers the full range manufacturers publish for PPS-CF. One honest caveat: some grades print best with a chamber close to PPS's glass transition (about 90–100 °C), and the printed part still leaves the machine only partly crystallized — plan an oven anneal for heat-critical parts whichever printer you use.

Epitum L is the right tool for production runs of solid PPS-CF parts: brackets, manifolds, fixtures. The 360 × 360 × 610 mm volume fits large housings in one piece, and the end-of-filament sensor pauses a long job when a spool runs out. Choose the Epitum JL when the geometry needs support you cannot break away — internal channels or enclosed cavities. Its JetSmart™ dual extrusion prints a soluble support such as VXL111, which lists PPS among its partner materials, from the second nozzle, and the blocking valve keeps the idle nozzle from oozing onto the part.

Applications

  • Pump, valve and manifold parts that see fuels, coolants, oils or acids
  • Electrical insulators, connector bodies and battery-pack brackets near heat sources
  • Fixtures for hot processes, plating lines or aggressive cleaning baths
  • Low-water-uptake parts that must hold tight dimensions in humid or wet service

Troubleshooting and tips

  • Anneal for heat resistance. Manufacturers publish very different schedules, from about 125–130 °C for several hours to 180–220 °C for 6–12 h. Ramp slowly, support thin walls, and expect small dimensional change.
  • Dry above 100 °C. PPS takes up little water, but surface moisture still causes pops and voids; most consumer dryers cannot reach the 100–140 °C that datasheets call for — use an oven.
  • Treat the filament as brittle. Keep the path from spool to extruder free of tight bends; a snapped strand mid-print is the most common failure.
  • Do not park hot. Lower the nozzle temperature during long pauses — PPS degrades and chars if left sitting in a 330 °C hot end.
  • Ventilate. PPS releases sulfurous odor when overheated; keep the room ventilated.

Available from MG World Tech: PPS CF 15, 0.75 kg spool, $159.19. Order or request a quote →

Frequently asked questions

Do I need a hardened nozzle for PPS carbon fiber?

Yes. Carbon fiber wears brass nozzles quickly, widening the orifice and changing extrusion width. Use hardened steel or another wear-resistant nozzle, 0.4 mm minimum; many manufacturers recommend 0.6 mm to avoid clogs.

Does PPS-CF need a heated chamber?

Not always. Some grades are formulated to print with no heated chamber; others recommend 60–90 °C. A warm chamber improves layer bonding and reduces warping on large parts. Epitum printers heat the chamber to 90 °C.

Should I anneal PPS-CF parts?

For heat-critical parts, yes. Annealing completes crystallization and raises stiffness and heat resistance. Follow your spool's datasheet: published schedules range from roughly 125 °C for 16 h to 180–220 °C for 6–12 h.

PPS-CF or PEEK — which should I print?

PPS-CF covers many parts specified for chemical resistance, low moisture uptake and heat up to around its deflection range, and it prints at lower temperatures. PEEK is tougher and rated for higher continuous temperatures. See our PEEK guide for that side of the comparison.