Materials guide · Basic

How to 3D print ABS: settings, warping control and high-speed ABS

ABS is the default engineering plastic of FFF printing: tough, machinable, easy to glue and paint, and good to roughly 85–100 °C. It is also the material that punishes a cold, open printer with warped corners and split layers. This guide gives typical settings across manufacturers, explains what changes with high-speed ABS, and covers first-layer adhesion in detail.

$46.63 ABS Performance · 1 kg spool · USD
Order / Request a quote

What ABS is — and when to choose it

Acrylonitrile butadiene styrene is an amorphous terpolymer: styrene gives stiffness and easy processing, acrylonitrile adds heat and chemical resistance, and dispersed butadiene rubber gives impact toughness. Compared with PLA and PETG it holds its shape at higher temperatures and is far easier to sand, machine, solvent-weld and paint.

Choose a related material when the part demands it: ASA for outdoor parts (the butadiene in ABS degrades in sunlight), ABS-CF for stiffness and less warping, flame-retardant PC/ABS for UL94 V-0 housings, or the specialty grades for static-sensitive electronics, food contact and medical devices.

Typical properties

PropertyTypical rangeTest method
Density1.04–1.10 g/cm³ISO 1183
Tensile strength, printed XY33–45 MPaISO 527
Tensile strength, printed Z29–32 MPaISO 527
Tensile modulus, XY1.7–2.3 GPaISO 527
Elongation at break, XY5–18 %ISO 527
Notched Charpy impact, XY18–22 kJ/m²ISO 179
Heat deflection, 1.8 MPa84–98 °CISO 75
Vicat softening94–104 °CISO 306
Glass transition101–105 °CDSC

Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).

Typical print settings

Nozzle temperature240–270 °C (high-speed grades toward the top)
Build plate80–110 °C; textured PEI, PC, or glass with adhesive
ChamberClosed and heated (Epitum: up to 90 °C); keep below the ~100 °C Tg
Print speed50–200 mm/s standard; up to ~300 mm/s high-flow grades
Part coolingOff to low; brief fan only for bridges and small overhangs
Drying70–80 °C · 6–8 h; store below 20 % RH
NozzleBrass is fine, ≥ 0.4 mm

Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.

High-speed ABS. High-flow grades are formulated to melt and solidify faster, so they survive the short residence time in the hot end at high speed. The real limit is volumetric flow: a 0.45 mm line at 0.25 mm layers and 300 mm/s needs about 34 mm³/s of fully molten plastic. Above what the hot end can melt you get underextrusion and weak layers. Print walls and top surfaces slower than infill, and check the heat-deflection figure on your spool's datasheet — some high-speed grades list a lower value than standard ABS.

First-layer adhesion

ABS shrinks as it cools, so the first layer has to hold the whole part against that pull for hours.

  • Surface. Textured PEI and PC sheets are the usual choices. On smooth PEI or glass, use an adhesive: it holds the part while hot and acts as a release layer once cool.
  • Glue-type adhesive. Water-based adhesives such as Magigoo Original go on as one thin, even layer, ideally on a cold bed, and need no drying time. The maker suggests 90–110 °C bed for ABS, ASA and HIPS.
  • Bed and chamber. 90–110 °C bed with the chamber closed and preheated before the first layer; a cold draft on the edges is enough to lift a corner.
  • Geometry. Use a 5–10 mm brim or corner "mouse ears" on large flat parts, and round sharp outside corners in CAD where possible.
  • Releasing parts. Let the bed cool — a 30–40 °C drop usually frees the part. Prying a hot part bends it. Water-based adhesives wipe off with a damp cloth.

Which Epitum: JL or L

For single-material ABS production the Epitum L ($8,299) is enough: the heated chamber (up to 90 °C) is the single most effective cure for warping, and the 360 × 360 × 610 mm volume takes large housings in one piece. An end-of-filament sensor pauses the job when a spool runs out.

Choose the Epitum JL ($9,899) for supports you cannot break away: pair ABS with HIPS (removed in limonene) or with soluble support. The idle nozzle is sealed by a mechanical valve and switches in under 0.5 s, with no wipe tower.

Both printers travel at up to 500 mm/s, but engineering ABS rarely benefits from that speed; plan for 50–200 mm/s, or up to about 300 mm/s with a high-flow grade.

Applications

  • Enclosures, housings and covers for electronics and instruments
  • Jigs, fixtures, gauges and assembly aids
  • Functional prototypes and parts to be painted, sanded or vapor-smoothed
  • Ducts, brackets and interior parts below about 85 °C

Troubleshooting and tips

  • Cracks between layers. Chamber too cold or fan too high. Close the chamber, turn the fan off, raise nozzle temperature 5–10 °C.
  • Corners lifting. Check bed temperature and adhesive, add a brim, and preheat the chamber before starting.
  • Bubbles or rough surfaces. Wet filament — dry before printing.
  • Fumes. ABS releases styrene and fine particles; print in an enclosed machine in a ventilated room or with filtered exhaust.

Available from MG World Tech: ABS Performance, 1 kg spool, $46.63; ABS FF, 1 kg spool, $49.79; Magigoo Original, 50 ml bottle, $21.95. Order or request a quote →

Frequently asked questions

What temperature should I print ABS at?

Typical manufacturer ranges are 240–270 °C at the nozzle and 80–110 °C on the bed, with part cooling off and the printer enclosed. Start mid-range and adjust in 5 °C steps.

Do I need an enclosure for ABS?

For anything larger than a few centimeters, yes. ABS shrinks as it cools; a closed, heated chamber keeps the part warm so corners do not lift and layers do not split.

How fast can you print ABS?

Standard ABS prints well at about 50–200 mm/s. High-flow grades are rated up to about 300 mm/s, but the hot end's volumetric flow sets the real limit — print outer walls slower to keep surface quality.

What is the best bed adhesive for ABS?

A textured PEI sheet or a thin layer of a glue-type adhesive on a 90–110 °C bed, plus a preheated chamber. See first-layer adhesion above for release and cleanup.

Related guides

Keep reading

All material guides →

Order ABS Performance or ask an engineer

Tell us about the part — we will confirm the material, settings and the right Epitum printer, and send a quote.

Request a quote