Materials guide · High-performance

How to 3D print PEI (ULTEM™-type)

Polyetherimide (PEI) is the amber, inherently flame-retardant polymer behind many aerospace and transport printed parts, sold under names such as ULTEM™ (a SABIC trademark). This guide covers the two common filament types, typical settings from several manufacturers, and what to expect on an Epitum printer.

What PEI is — and when to choose it

PEI is an amorphous high-temperature thermoplastic. It has no melting point and no crystallization to manage. Parts come off the printer with their final structure, which makes PEI the most predictable of the high-performance polymers. It is inherently flame-retardant, low in smoke and stiff up to its glass transition. Filaments come in two families:

  • 9085-type is a PEI/PC blend with Tg around 177–186 °C. It is a little tougher and easier to print, and it is the usual choice for aerospace interiors, where makers publish flame, smoke and toxicity (FST) testing to 14 CFR 25.853.
  • 1010-type is neat PEI with Tg around 209–217 °C. It is stiffer and more heat-resistant, but needs a hotter nozzle and is more prone to warping.

Choose PEI over PC or flame-retardant PC/ABS V-0 when the part sees 150–200 °C or must meet aerospace FST. Move to PEEK or PEKK when you need semi-crystalline chemical resistance above 200 °C. PEI resists fuels and many fluids, but some solvents can stress-crack it.

Typical properties

PropertyTypical rangeTest method
Glass transition (Tg)177–186 °C (9085-type) · 209–217 °C (1010-type)DSC / ASTM D7426
HDT at 0.45 MPa157–178 °C (9085-type) · ≈ 208–214 °C (1010-type)ISO 75 / ASTM D648
Tensile strength, XY55–90 MPaISO 527 / ASTM D638
Tensile modulus, XY2.0–3.0 GPaISO 527 / ASTM D638
Elongation at break3–7 %ISO 527 / ASTM D638
Tensile strength, Z (through layers)≈ 40 MPa on a published 9085-type sheet, roughly 60 % of XYASTM D638
Density1.27–1.34 g/cm³ISO 1183
Flammability (base resin)UL94 V-0; 9085-type FST tested to 14 CFR 25.853 by some makersUL94 / FAR 25.853

Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).

Typical print settings

Nozzle temperature350–385 °C (9085-type) · 370–400 °C (1010-type) (Epitum: up to 430 °C)
Build plate120–160 °C (Epitum: up to 150 °C)
ChamberEnclosed, ≥ 80–90 °C; up to 170–180 °C on dedicated systems (Epitum: up to 90 °C)
Print speed20–30 mm/s
Part coolingOff to 25 %
Drying120 °C · 4–6 h (9085-type); up to 150 °C · 4 h (1010-type)
Nozzle430 °C-rated, ≥ 0.4 mm

Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.

The Epitum hot end reaches 430 °C, comfortably above both PEI types. The chamber is the limit to be honest about. Epitum heats it actively to 90 °C. Several filament makers ask only for an enclosed chamber above about 80–90 °C, while dedicated PEI systems run their build environments close to Tg; one maker lists 170–180 °C. A 90 °C chamber leaves a gap of 90–125 °C to Tg. Small and medium parts print well; as size and height grow, so do warping and interlayer delamination. 9085-type is the better starting point at 90 °C.

Which Epitum: JL or L

For PEI parts printed in one material, the Epitum L is the straightforward choice. The Epitum JL adds a second nozzle, sealed by its blocking valve when idle. Use it to keep a nozzle dedicated to PEI, to print a second material, or to run a breakaway support. Soluble supports for PEI and PAEK exist but are specialized high-temperature products; see the general soluble-support guide. We review PEI parts individually and tell you plainly if a part needs a hotter machine.

Applications

  • Aircraft-interior brackets, ducts, clips and panels prototyped or produced in 9085-type
  • Rail and transport parts with fire, smoke and toxicity requirements
  • Electrical insulators, connector bodies and housings near hot components
  • Fixtures and jigs for hot processes, 1010-type for the highest temperatures

Troubleshooting and tips

  • Dry it hotter than you think. PEI is hygroscopic and needs 120–150 °C, which most consumer dryers cannot hold; check that your spool tolerates the temperature. Wet PEI foams, strings and prints weak layers.
  • Bed adhesion. Makers list smooth or textured PEI sheet, polyimide (Kapton-type) tape, or a high-temperature adhesive on a 120–160 °C plate. Release the part only after the plate cools.
  • Corners lifting. Use a brim, round sharp corners, and preheat the closed chamber before printing. Keep the door shut until the job is done.
  • Layers splitting on tall parts. Slow down and keep part cooling off. Printing one part at a time keeps layer times short, which helps bonding.
  • No anneal needed. Amorphous PEI has nothing to crystallize. Optional stress-relief bakes must stay well below Tg.

Not in our standard catalog. Talk to an engineer about your PEI part: contact us →

Frequently asked questions

What is the difference between ULTEM™ 9085 and 1010-type filament?

9085-type is a PEI/PC blend (Tg ≈ 177–186 °C), tougher and easier to print, used for aerospace FST parts. 1010-type is neat PEI (Tg ≈ 209–217 °C), stiffer and more heat-resistant, and needs a hotter nozzle.

Can you print PEI with a 90 °C chamber?

Yes, for small and medium parts; several filament makers ask only for an enclosed chamber above about 80–90 °C. Large, tall or 1010-type parts are more likely to warp or delaminate, and run better on hotter machines. Send us the part for an honest assessment.

Does printed PEI need annealing?

No. PEI is amorphous, so there is no crystallization step, unlike PEEK or PEKK.

What bed surface works for PEI?

Makers list PEI sheet, polyimide tape or a high-temperature adhesive, with the plate at 120–160 °C.

Related guides

Keep reading

All material guides →

Talk to an engineer about your PEI part

Send us the drawing, the load case and the service temperature — we will tell you honestly whether the Epitum envelope fits the part.

Talk to an engineer