Materials guide · Engineering

How to 3D print polypropylene (PP)

Polypropylene is the lightest common engineering plastic, shrugs off most acids, bases and cleaning agents, and survives repeated flexing. It is also notorious for not sticking to anything — including the print bed. This guide covers the bed surfaces that work, warping control and typical settings.

$66.04 PP4 · 0.75 kg spool · USD
Order / Request a quote

What polypropylene is — and when to choose it

PP is a semicrystalline polyolefin. Choose it for parts that flex repeatedly (living hinges, snap-fits, clips), parts that meet chemicals (lab ware, fluid-handling fixtures, battery and cleaning-agent contact), and parts that must be light — at about 0.9 g/cm³ it floats on water. It is soft and flexible compared with ABS and stiffens only with fiber: carbon-fiber PP is far stiffer and warps much less.

The same low surface energy that makes PP chemically inert makes it hard to bond: glue and most bed surfaces do not hold it, and it welds best to other polypropylene.

Typical properties

PropertyTypical rangeTest method
Tensile strength (printed, XY)10–25 MPaISO 527 / ASTM D3039
Tensile or flexural modulus0.25–1.4 GPaISO 527 / ISO 178
Elongation at break (XY)20% to over 800% (grade-dependent)ISO 527
Heat deflection, 0.45 MPa54–65 °CISO 75
Melting point130–165 °C (copolymer vs homopolymer)DSC
Density0.89–0.91 g/cm³ISO 1183

Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).

Typical print settings

Nozzle temperature205–250 °C
Build plate60–100 °C on PP tape, PP sheet or PP adhesive
ChamberClosed, warm (Epitum: up to 90 °C)
Print speed20–50 mm/s
Part cooling0–50%
DryingUsually not needed; 60 °C · 4–16 h if wet
NozzleBrass or steel, ≥ 0.4 mm

Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.

The bed surface matters more than the temperature. PP packing tape suits small parts; a PP sheet fixed to the plate suits large ones; PP-specific adhesives on a smooth plate are the third option. General-purpose glues for ABS or PLA are not made for PP. Too hot a bed can fuse the part to a PP sheet — lower it in steps.

Which Epitum: JL or L

The Epitum L is the natural fit: PP parts are almost always single-material, and the heated chamber (up to 90 °C) slows cooling and cuts warping on large flat parts. The Epitum JL makes sense when one machine also runs other materials — keep one nozzle on PP. PP prints at moderate speeds, far below the 500 mm/s travel peak, so large parts run for many hours — the end-of-filament sensor pauses the job if a spool runs out, and on the JL with PP in both nozzles, Hot Swap mode carries on from the second one.

Applications

  • Living hinges, snap-fit lids and clips
  • Lab equipment, trays and containers for acids, bases and solvents
  • Fluid-handling fixtures, ducts and tank fittings
  • Lightweight covers, protective cases and packaging prototypes

Troubleshooting and tips

  • Part won't stick. Clean the PP tape or sheet with isopropyl alcohol, add a brim, slow the first layer. Glass, bare PEI and blue tape rarely hold PP.
  • Corners lift or the part bows. Close and heat the chamber, add a wide brim, round sharp corners and avoid large solid floors.
  • Living hinges crack. Print the hinge flat, with extrusion lines running across the fold, and never place a Z layer boundary along the hinge line.
  • Chemicals. PP resists most acids, bases and alcohols but swells in aromatic and chlorinated solvents and is attacked by strong oxidizers — test your medium.
  • Stringing. Lower nozzle temperature and use longer, slower retraction.
  • Holes and fits come out small. PP shrinks more than ABS. Print a test coupon, measure it and compensate holes and mating features in the slicer before running the batch.

Available from MG World Tech: PP4, 0.75 kg spool, $66.04. Order or request a quote →

Frequently asked questions

What bed surface do you need to print polypropylene?

A polypropylene surface: PP packing tape, a PP sheet fixed to the plate, or a PP-specific adhesive. PP bonds best to itself; glass and bare PEI rarely hold it.

Why does polypropylene warp so much?

PP is semicrystalline and shrinks strongly as it crystallizes. A closed, heated chamber, a wide brim and rounded corners help; carbon-fiber PP warps much less.

Can you 3D print living hinges in PP?

Yes — PP's fatigue resistance makes it the classic living-hinge material. Print the hinge flat with lines across the fold and keep it thin.

Does PP filament need drying?

Rarely: PP absorbs very little water. If a spool has sat in humid air and prints with bubbles, dry it at about 60 °C for several hours.

Related guides

Keep reading

All material guides →

Order PP4 or ask an engineer

Tell us about the part — we will confirm the material, settings and the right Epitum printer, and send a quote.

Request a quote