What PMMA casting filament is — and when to choose it
Polymethyl methacrylate (PMMA) is a clear acrylic. At casting temperatures it depolymerizes and burns, which is why PMMA is also used for casting patterns in industrial powder-bed printing. One article notes that PMMA “burns to ash, leaving very little residue behind” in casting.
For FDM, the picture is more mixed. We found PMMA filaments with published print settings, but none of the PMMA filament datasheets we reviewed stated ash content or a burnout schedule. By contrast, a widely used PVB-based casting filament publishes a full datasheet, claims 0.003 % ash and recommends a high-temperature burnout. If your foundry needs documented numbers, PVB is easier to qualify today; if you already cast PMMA patterns, PMMA filament is a logical extension. In both cases, run a burnout trial before committing to production. For softer, lower-temperature patterns use wax filament.
Typical properties
| Property | Typical range | Source type |
|---|---|---|
| PMMA density | 1.17–1.20 g/cm³ | Filament pages, article |
| PMMA softening / HDT | ≈ 77 °C Vicat-type (modified acrylic); 82 °C HDT at 1.8 MPa (PMMA/PC blend) | Filament pages |
| PMMA tensile strength | ≈ 51 MPa (one modified grade) | ASTM D638 |
| PVB casting filament Tg | ≈ 70 °C | DSC, 10 °C/min |
| PVB casting filament density | ≈ 1.1 g/cm³ | ISO 1183 |
| PVB water uptake | ≈ 2 % at equilibrium (70 % RH) | Datasheet curve |
| Ash after burnout | PVB maker: 0.003 %; PMMA filament: not published | Maker claim |
Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).
Typical print settings
| Nozzle temperature | PMMA 220–265 °C; PVB casting filament 190–220 °C (Epitum: up to 430 °C) |
|---|---|
| Build plate | PMMA 90–120 °C; PVB 25–70 °C |
| Chamber | Enclosed, heating off or low; do not use 90 °C (Epitum: heating optional) |
| Print speed | PMMA 30–50 mm/s; PVB up to 50–200 mm/s by its maker |
| Part cooling | PMMA 0–20 %; PVB on |
| Drying | PMMA 70 °C · 3 h or more; PVB 50 °C · 12 h |
| Nozzle | Brass or hardened, 0.3 mm or larger |
Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.
PMMA prints hotter than PVB casting filament and shrinks as it cools, so sources suggest slow printing (about 30–50 mm/s), little or no part cooling and an enclosure that moderates drafts. They do not specify a chamber temperature. PMMA softens between roughly 77 °C (one modified grade) and about 82 °C (a PMMA/PC blend), so a chamber at the Epitum maximum of 90 °C is not advisable: it would soften the pattern. Keep chamber heating off or low and use a closed door as a draft shield. PVB casting filament needs no enclosure at all, and its glass transition is about 70 °C.
From pattern to metal: the casting workflow
- Print. Use sparse infill. FDM pattern guidance from one printer maker says a sparse fill reduces material, prevents shell damage and minimizes ash; their ABS pattern left about 0.021 % ash.
- Sprue and tree. Attach the pattern to a wax sprue system.
- Invest. Build the ceramic shell and vent it; venting speeds combustion.
- Burn out. PVB maker: about 1,100–1,200 °C for complete burnout, or a longer hold at lower temperature. A foundry-industry paper warns that fused-silica shells burned out at 1,800 °F (about 980 °C) or above form cristobalite that cracks on cooling, so many foundries keep preheat at 1,500 °F (about 815 °C) or less. Follow your shell supplier's schedule.
- Cast, wash and finish. Wash residual ash from the shell cavity before pouring.
Who uses it: investment foundries and engineering shops for prototype or low-volume castings, jewelers and dental casters working from burnout resins, and designers who need a pattern without tooling.
Surface finishing
PMMA dissolves in acetone, and filament makers describe acetone smoothing and polishing as the way to a smooth or even transparent surface; test on a scrap, because acetone also attacks fine detail. PVB is smoothed with isopropyl alcohol, which its maker says carries over to the cast model. Sanding works on both before the pattern is invested.
Which Epitum printer: JL or L
Epitum L prints both families comfortably: the 430 °C hot end and 150 °C bed far exceed what they need, and the 360 × 360 × 610 mm volume holds patterns for a full tree. The Epitum JL can add a soluble support from its second nozzle; one PVB maker recommends a water-soluble support for its filament (see the soluble-support guide). Leave the chamber unheated or low.
Troubleshooting and tips
- Ash after burnout. Reduce infill, add vents and extend the hold; thick solid sections leave the most.
- Stringing and bubbles. PVB absorbs about 2 % water at equilibrium; dry it (about 50 °C for 12 h per its maker). PMMA is dried at about 70 °C for 3 h or more.
Not in our standard catalog. Talk to an engineer about your casting patterns: contact us →
Frequently asked questions
Does PMMA filament burn out without ash?
Not literally. Plastic patterns always leave a trace; for FDM ABS patterns one maker measured about 0.021 %, and a PVB maker claims 0.003 %. We found no published ash figure for PMMA filament itself, so test it.
How does PMMA compare with wax?
Wax-like filament prints cool and melts out at modest temperatures, but is brittle. PMMA prints hotter, is stiffer, and burns out at high temperatures, so shells and burnout schedules matter more. See the wax guide.
Is PolyCast-type filament PMMA?
No. The PolyCast type is PVB (polyvinyl butyral), a different polymer with a lower print temperature.
Can I smooth PMMA patterns?
Acetone smoothing and polishing are described by PMMA filament makers. Test it first, as it can soften small details.