Materials guide · Support

Soluble support for PLA, PETG and TPU

For PLA, PETG and flexible TPU, a dissolvable support turns impossible overhangs and internal cavities into routine prints. The three common types behave differently with each material — this guide compares them and covers the settings that keep the interface bonded.

$181.50 VXL90 · 0.5 kg spool · USD
Order / Request a quote

Which dissolvable support for lower-temperature materials

PLA, PETG and TPU print at modest temperatures in a cool or unheated chamber, so the support does not need to survive heat. It needs to bond to the model, stay dimensionally stable and dissolve without harming the part.

  • PVA dissolves in water and pairs well with PLA and TPU. It is very hygroscopic, and makers disagree on PETG: some list it as compatible, others leave it out.
  • BVOH dissolves readily, even in cold water, and its makers list adhesion to PLA, PETG, ABS, ASA and TPU — the broadest match in this class.
  • Removal-agent soluble copolymers dissolve in a bath of water and an alkaline agent. They tolerate humidity better than PVA and BVOH.

The catalog support offered here is listed for PLA, PETG, ABS, ASA and TPU, and is removed in a water bath with a removal agent. For nylon, PC or PPS parts in a hot chamber, see soluble support for engineering plastics.

Typical properties by support type

Support typeRemoved withPairs with · notes
PVAWater; warm water speeds itPLA, TPU, nylon; PETG varies by grade · Tg ≈ 58–60 °C
BVOHWater, even coldPLA, PETG, ABS, ASA, TPU · Tg ≈ 68 °C
Removal-agent solubleWater + alkaline agent, heated bathPer grade · less moisture-sensitive

Typical published values across manufacturers, measured on test specimens; check your spool’s datasheet. Printed parts are usually weaker between layers (Z) than along them (XY).

Typical print settings

Nozzle temperature190–225 °C (PVA 215–225 °C, BVOH 190–220 °C)
Build plateSet for the model material (25–60 °C for the support itself)
ChamberOff or cool for PLA, PETG, TPU; modest for ABS/ASA (Epitum: up to 90 °C)
InterfaceZ gap 0 mm; 2–4 dense interface layers
Print speed30–40 mm/s for support
Part coolingOn for PLA; BVOH tolerates 75–100%
DryingBVOH 50 °C · 4 h; PVA up to 80 °C · 12 h if wet

Starting point compiled from manufacturers’ recommendations — fine-tune with the Printoformer material profile for your spool, nozzle and part geometry.

Keep the chamber heat off for PLA: both PLA and PVA soften around 55–60 °C, and a warm chamber causes heat creep and drooping overhangs. ABS and ASA want warmth, so check the support grade’s limit before heating the chamber.

Why it needs the Epitum JL

Support and model must come from separate nozzles, so the single-extruder Epitum L cannot print soluble support. The Epitum JL switches between its two nozzles in under 0.5 s, and a mechanical valve seals the idle one so it cannot ooze onto the part. No wipe tower is printed, which matters when the support costs more per kilogram than the model.

Applications

  • TPU seals, bellows and grips — breaking support off a flexible part tears or stretches it
  • PLA and PETG prototypes with internal channels and enclosed cavities
  • Print-in-place hinges and assemblies
  • Display models with clean downward-facing surfaces

Troubleshooting and tips

  • PETG lifts off the interface: PETG bonds less readily than PLA. Set the Z gap to 0, slow the first model layer over the support, raise the nozzle 5–10 °C there, and use a support type its maker lists for PETG.
  • Bubbling, stringy support: it is wet. Dry it and print from a dry box.
  • Warped TPU after soaking: keep the bath warm, not hot, and dry the part flat.
  • Bed adhesion: for PLA, PETG and TPU see first-layer adhesion.
  • Disposal: follow local wastewater rules; one BVOH maker sets a daily drain limit.

Available from MG World Tech: VXL90, 0.5 kg spool, $181.50; VXL EX 1000g, 1 kg spool, $73.15. Order or request a quote →

Frequently asked questions

What is the best soluble support for PETG?

BVOH is the most widely listed for PETG; PVA compatibility varies by brand. Whatever you use, print the interface with zero Z gap and test a small part first, because PETG bonds less readily than PLA.

PVA or BVOH — which is better?

BVOH dissolves readily, even in cold water, and bonds to a broader range including PETG, ABS and ASA. PVA is common and works well with PLA and TPU. Both absorb moisture quickly.

How long does dissolvable support take to dissolve?

From under an hour to many hours, depending on support volume, water temperature and agitation. Remove bulk support first, use warm water and stir or circulate the bath.

Can I print soluble support for TPU?

Yes — it is one of the best uses, because breakaway support distorts flexible parts. PVA and BVOH are both listed for TPU; print TPU slowly and keep the bath warm, not hot.

Related guides

Keep reading

All material guides →

Order VXL90 or VXL EX 1000g or ask an engineer

Tell us about the part — we will confirm the material, settings and the right Epitum printer, and send a quote.

Request a quote